MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Murtfeldt Murylon® HT Nylon 46
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes: The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entire temperature range far better than other Murylon® types.

Special Properties:
• Highly wear-resistant and good slide properties, especially at high temperatures
• Good resistance to thermal aging
• High creep resistance

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PA 46
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183-1
Moisture Absorption at Equilibrium 2.8 %
@Temperature 23.0 °C
50% RH
Water Absorption at Saturation 9.5 %
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ISO 2039-2
Hardness, Shore D 80DIN 53505
Ball Indentation Hardness 165 MPaISO 2039-1
Tensile Strength, Yield 55.0 MPa50% RH; ISO 527-1/-2
 105 MPadry; ISO 527-1/-2
Elongation at Break 25 %dry; ISO 527-1/-2
 >= 100 %50% RH; ISO 527-1/-2
Creep Strength 7.50 MPastress leading to 1% elongation; 50% RH; ISO 899-1
 22.0 MPastress leading to 1% elongation; dry; ISO 899-1
Modulus of Elasticity 1.35 GPa50% RH
 3.40 GPadry
Compressive Yield Strength 23.0 MPa
@Strain 1 %
dry; ISO 604
 45.0 MPa
@Strain 2 %
dry; ISO 604
 94.0 MPa
@Strain 5.0 %
dry; ISO 604
Charpy Impact Unnotched NBISO 179-1/1eU
 NBISO 179
Charpy Impact, Notched 8.00 kJ/m²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.34
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cm50% RH; IEC 60093
 >= 1.00e+14 ohm-cmdry; IEC 60093
Surface Resistance >= 1.00e+12 ohm50% RH; IEC 60093
 >= 1.00e+13 ohmdry; IEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
dry; IEC 60250
 3.5
@Frequency 100 Hz
dry; IEC 60250
 3.8
@Frequency 1e+6 Hz
50% RH; IEC 60250
 7.4
@Frequency 100 Hz
50% RH; IEC 60250
Dielectric Strength 15.0 kV/mm50% RH; IEC 60243-1
 25.0 kV/mmdry; IEC 60243-1
Dielectric Loss Index 0.0090
@Frequency 100 Hz
dry; IEC 60250
 0.019
@Frequency 1e+6 Hz
dry; IEC 60250
 0.060
@Frequency 1e+6 Hz
50% RH; IEC 60250
 0.13
@Frequency 100 Hz
50% RH; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
Melting Point 290 °CISO 11357-1
Maximum Service Temperature, Air 130 °C
@Time 7.20e+7 sec
 150 °C
@Time 1.80e+7 sec
 200 °C
@Time <=86400 sec
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 80.0 °CISO 11357-1
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorAuburn

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe PA 46 Nylon 46
Overview of materials for Nylon 46, Unreinforced
LATI Latamid 66 PA 66
Alclad Aluminum 7075-T6, T651
Akro-Plastic Akromid® A3 1 black (2417) PA 66 Dry

PMURT932 / 156579

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.