MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Test specimens were transfer molded and post cured 4 hours at 175°C.

A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It is formulated with a unique filler system that reduces the expansion coefficient without compromising moldability. Ultra low stress properties; Outstanding moldability (good mold filling, low wire sweep, fast cycles and good hot hardness); Superior reliability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.88 g/cc0.0679 lb/in³
Water Absorption 0.0034 %0.0034 %
Viscosity 8500 cP
@Temperature 175 °C
8500 cP
@Temperature 347 °F
Automatic orifice Viscosity
Linear Mold Shrinkage 0.0025 cm/cm0.0025 in/in
Spiral Flow 95.0 cm37.4 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
Flexural Strength 121 MPa17500 psi
Flexural Modulus 14.0 GPa2030 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
Dielectric Strength 16.0 kV/mm406 kV/in
Dissipation Factor 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
Arc Resistance 180 sec180 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.5 µm/m-°C
@Temperature 20.0 °C
6.94 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
36.1 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 166 °C331 °F
Flammability, UL94  V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 185 °C338 - 365 °FMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond LED405Med One component, nanosilica filled LED curable system
Hexcel® HexPly® F263 Epoxy Resin
Armstrong X-6/E Epoxy Adhesive
Solvay LTM® 12 Epoxy Resin
NuSil Lightspan™ LS-8941 Silicone, Optical Adhesive Elastomer

PCOOK337 / 21433

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.