MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Features:

  • Chemical Resistance, Good
  • Colorability, Good
  • Elasticity, High
  • Electrically Insulating
  • Flame Retardant
  • Flexibility, Good
  • Hardness, Low
  • Heat Stabilized
  • Ozone Resistant
  • Processability, Good
  • Soft
  • UV Resistance, Good
  • Forms:

  • Pellets
  • Processing Method:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 0.890 g/ccASTM 792
    Water Absorption 0.040 %ASTM D570
    Melt Flow 30 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     52.6 g/10 min
    @Load 5.00 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 3.0ASTM D2240
     6.510 seconds; ASTM D2240
    Tensile Strength, Ultimate 321 psiASTM D638
    Tensile Strength, Yield 30.0 psiat 100%; ASTM D412
     250 psiElastic; ASTM D412
    Elongation at Break 750 %Elastic; ASTM D412
     830 %ASTM D638
    Tear Strength 51.0 pliASTM D624
     
    Processing PropertiesOriginal ValueComments
    Middle Barrel Temperature 410 °F
    Front Barrel Temperature 440 °F
    Nozzle Temperature 455 °F
    Mold Temperature 125 °F
    Drying Temperature 125 °F
    Dry Time 2 - 4 hour
    Injection Pressure 500 - 700 psi
    Back Pressure 50.0 psi
    Screw Speed 40 rpm
     
    Descriptive Properties
    Clamp Tonnage1.5-2.5 tons/in2
    Injection RateFast
    Suggested Max Regrind0.5

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
    ELASTO UK Dryflex® 500300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Translucent
    CPT C-Flex® R70-190 Opaque Biocompatible TPE
    Covestro DESMODUR® TD636 + BAYTEC® XL TMP-TIPA + PLASTICIZER V10 (SD6-40 Catalyst), 20 A Polyurethane, TDI- Ester
    Colorite Polymers Flexchem 3551-02 Vinyl Compound

    PMULTI005 / 53909

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.