HI5748 is an UV light stabilized high density polyethylene for injection molding. HI5748 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applications: Crates and containers, Pails, Pallets, Bins, Caps & closures and other technical parts. Advantages: Outstanding UV resistance, Excellent stiffness Information provided by Lotte Advanced Materials. |