MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ExxonMobil Escorene™ LD 783.CD Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Escorene Ultra LD 783.CD is a 31.4% VA copolymer that is suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and very low modulus. LD 783.CD contains an additive package to improve pellet flowabiltiy and handling.

Availability: North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Crosslinkable Compounds
  • Extrusion Compounds
  • Molding Compounds
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ExxonMobil method
Vinyl Acetate Content 31.4 %31.4 %ExxonMobil method
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 190 °C
43 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55
@Time 15.0 sec
55
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 3.03 MPa440 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 12.4 MPa1800 psiASTM D790
Dart Drop, Total Energy  10.8 J
@Temperature 22.8 °C
8.00 ft-lb
@Temperature 73.0 °F
ASTM D3763
 29.8 J
@Temperature -40.0 °C
22.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 57.8 °C<= 136 °FPeak Melting Point; ExxonMobil method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 30 EVA + PE Foam
Eurofoam Evacell EVA 100 EVA + PE Foam
Dow Elvax® 3169Z Ethylene Vinyl Acetate
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer

PEX99071 / 175307

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.