MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta EndurX™ BP11NPG Phenolic Cotton Laminate Sheet, Graphite Lubricated
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should not be used where this is detrimental to the application.

Key Words: Cotton, Phenolic, Micarta, Graphite Lubricant
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Moisture Absorption 2.20 %Condition A; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength 7000 psi
@Thickness 3.17 mm
Condition A, Crosswise; ASTM D638
 10000 psi
@Thickness 3.17 mm
Condition A, Lengthwise; ASTM D638
Flexural Strength 15000 psi
@Thickness 1.57 mm
Condition A, Crosswise; ASTM D790
 19000 psi
@Thickness 1.57 mm
Condition A, Lengthwise; ASTM D790
Flexural Modulus 1000 ksi
@Thickness 1.57 mm
Condition A, Crosswise; ASTM D790
 1200 ksi
@Thickness 1.57 mm
Condition A, Lengthwise; ASTM D790
Compressive Strength 38000 psi
@Thickness 12.7 mm
Condition A, Flatwise; ASTM D695
Shear Strength 13000 psi
@Thickness 1.57 mm
Condition A, Perpendicular; ASTM D732
Adhesive Bond Strength 1800 psi
@Thickness 12.7 mm
Condition A, Bonding Strength; ASTM D229
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 12.7 mm
Condition E-48/50, Crosswise; ASTM D256
 1.70 ft-lb/in
@Thickness 12.7 mm
Condition E-48/50, Lengthwise; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Thickness 3.17 mm
X-axis; IPC-TM 650-2.4.24
 24.0 µm/m-°C
@Thickness 3.17 mm
Y-axis; IPC-TM 650-2.4.24
UL RTI, Mechanical without Impact 125 °CUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
Condition A
 
Descriptive Properties
SubstrateCotton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM231 / 280547

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.