MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Aluminum Bronze, UNS C95200, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Acid-resisting pumps, bearings, gears, valve seats, guides, plungers, pump rods, bushings.

Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9A

Typical data for sand-cast test bars. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.6%

Key Words: Aluminum bronze, ASTM B148, ASTM B148-9A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.64 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 1253000 kg
Hardness, Rockwell B 64
Tensile Strength, Ultimate 550 MPaas cast
 390 MPa
@Temperature 315 °C
 400 MPa
@Temperature 300 °C
 450 MPa
@Temperature 250 °C
 490 MPa
@Temperature 200 °C
 525 MPa
@Temperature 150 °C
 550 MPa
@Temperature 100 °C
 570 MPa
@Temperature 25.0 °C
 570 MPa
@Temperature 50.0 °C
Tensile Strength, Yield 185 MPaas cast
 185 MPa
@Strain 0.5 %,
Temperature 150 °C
 185 MPa
@Strain 0.5 %,
Temperature 200 °C
 190 MPa
@Strain 0.5 %,
Temperature 250 °C
 190 MPa
@Strain 0.5 %,
Temperature 100 °C
 195 MPa
@Strain 0.5 %,
Temperature 300 °C
 195 MPa
@Strain 0.5 %,
Temperature 315 °C
 200 MPa
@Strain 0.5 %,
Temperature 50.0 °C
 205 MPa
@Strain 0.5 %,
Temperature 25.0 °C
Elongation at Break 35 %in 50 mm
Reduction of Area 3.0 %
@Temperature 150 °C
 23 %
@Temperature 315 °C
 24 %
@Temperature 300 °C
 30 %
@Temperature 250 °C
 32 %
@Temperature 200 °C
 38 %
@Temperature 100 °C
 43 %
@Temperature 50.0 °C
 46 %
@Temperature 25.0 °C
Creep Strength 54.0 MPa
@Temperature 315 °C
for 0.00001%/h
 145 MPa
@Temperature 230 °C
for 0.00001%/h
Modulus of Elasticity 105 GPa
Poissons Ratio 0.31
Fatigue Strength 150 MPa
@# of Cycles 1.00e+8
rotating beam
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
Izod Impact 40.0 J
@Temperature -18.0 - 38.0 °C
Charpy Impact 27.0 J
@Temperature -18.0 - 38.0 °C
Keyhole
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000144 ohm-cm
Magnetic Permeability 1.2at 16,000 A/m
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 50.0 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1045 °C
Solidus 1040 °C
Liquidus 1045 °C
Shrinkage 2.0 %Patternmaker's Shrinkage
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 - 745 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 8.5 - 9.5 %
Copper, Cu >= 86 %
Iron, Fe 2.5 - 4.0 %
Other, total <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 230-N Cast UNS C95800 Nickel Aluminum Bronze
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze
Aluminum Bronze, UNS C95300, Casting Alloy, As Cast
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast

MC95200b1 / 11961

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.