MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Krytox® MIL PRF-27617 240 AB PFPE Lubricant  (discontinued **)
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Fuel and oxidizer resistant, aircraft and instrument grease.

This product passes tests on film stability, corrosion on steel, resistance to distilled water, and resistance to 50/50 distilled water/ethanol. This product offers no reaction to liquid oxygen impact after 20 impacts at 43.3 in.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 77.8 cStBase Oil
Evaporation Loss 10.1 %ASTM D2595
 
Mechanical PropertiesOriginal ValueComments
Oil Separation 14.2 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Corrosion on Copper1b
High Temperature Bearing PerformanceStopped at 1320 hr1500 hr min. at 10,000 rpm, 204°C
NATO Number398
Oxidation Stability (psi)0.5
Solubility in Fuel (%)0.3
Standard NLGI Penetration Grade2
Water Washout Characteristics (%)0.25

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Krytox® NRT 8904 PFPE Lubricant
Chemours Krytox® CORR 226 FG PFPE Corrugator Grease
Chemours Krytox® NRT 8906 PFPE Lubricant
Chemours Krytox® 1645 Vacuum Service Fluid
Chemours Krytox® 16256 Vacuum Pump Fluid

WDUPJ936 / 162470

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.