MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Silpak SP-328-12 Rigid Polyurethane Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SP-328-12 A/B is a two-component, self-skinning, rigid, closed cell, water blown, polyurethane rigid foam system. SP-328 foam can be hand mixed or machine dispensed. Small batch mixes are easily achieved using fast, aggressive mixing methods with larger mixes better achieved using a high shear mixing blade (Jiffy Mixer). Once cured, parts can be stained, sanded, or painted shortly after demolding.

Features:

  • 1:1 volume mix
  • Excellent Flow
  • Self-skinning
  • Fast de-molding times
Applications: Recommended for any application where a high-density, light-weight part is required:
  • Furniture production
  • Hollow, light weight furniture parts
  • Picture frames
  • Duck Decoys
  • Floats

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccPart B
 1.20 g/cc1.20 g/ccPart A
Density 1.44 g/cc0.0519 lb/in³
Viscosity 150 - 190 cP150 - 190 cPInitial, Part A
 900 - 1300 cP900 - 1300 cPInitial, Part B
Storage Temperature 17.8 - 30.0 °C64.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.07 MPa300 psi
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 min0.0167 hourCream Time
 2.50 min0.0417 hour
 10.0 - 15.0 min0.167 - 0.250 hourDemold Time
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorLight brown
Expansion Rate (volume)<6 times mixed volume
Mix Ratio50 A : 50 Bby volume
 52% A : 48% Bby weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSILPAK012 / 318649

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.