Adflex Z 108 S is a reactor TPO (thermoplastic polyolefin) manufactured using the proprietary Catalloy process technology from LyondellBasell. Adflex Z 108 S features a very high softness, a very low flexural modulus and a high melt flow rate. It is used for injection molding, impact modification, extrusion coating, soft compounding, film and fiber applications. It is also selected for the modification of polypropylene homopolymer and random copolymer without altering the transparency. The grade is available in natural pellet form. Commercial: Active Availability Europe; North America; South & Central America. Application: Carpet Backing; Filament Yarn; Hygiene Nonwoven; Impact Modification; Pipe Coating; Roofing Underlayment; TPO Foils and Skins Market Flexible Packaging; Industrial, Building & Construction; Textile Processing Method Cast Film; Compounding; Continuous Filament/Spinning; Extrusion Coating; Injection Molding; Spunbond. Attribute: High Elongation; High Flow; Low Hardness; Low Temperature Impact Resistance; Narrow Molecular Weight Distribution.Information provided by LyondellBasell. |