MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2080815P1 Silver Flexographic Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and good conductivity.
Testing was carried out on a Timsons T-Flex 508 and Nilpeter FB-3300.
Substrate: Polyester, PVC, BOPP, Cellophane, Paper or Cellulosic Board

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 66 - 68 %
@Temperature 700 °C
66 - 68 %
@Temperature 1290 °F
Viscosity 800 - 1000 cP
@Shear Rate 50 1/s,
Temperature 25.0 °C
800 - 1000 cP
@Shear Rate 50 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000065 ohm-cm0.000065 ohm-cmprinted onto 125µm PET film using 18cm3m-2 anilox
Surface Resistivity per Square  0.025 - 0.030 ohm
@Thickness 0.0250 mm
0.025 - 0.030 ohm
@Thickness 0.000984 in
printed onto 125µm PET film using 18cm3m-2 anilox
 0.15 - 0.165 ohm
@Thickness 0.00400 mm
0.15 - 0.165 ohm
@Thickness 0.000157 in
Printed onto 125µm PET film using 18cm3m-2 anilox
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGELZ9081 / 139394

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.