Hostacom HKP 2400D NAT is a mineral filled PP homopolymer with medium melt flow rate. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Appliances Market: Electrical / Electronics Processing Method: Injection Molding Attribute: Medium Flow Information provided by LyondellBasell. |