MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

RAMPF RAKU® TOOL InnoClear™ OC-5030 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Water clear, semi-flexible polyurethane elastomer

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
  • Low viscosity and uses materials that have excellent U.V. resistant qualities
Applications:
  • For hand-batch or vacuum assisted processing
Cure 1: 24 hours at 77°F + 16 hours at 180°F
Cure 2: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³Resin; ASTM D-792
 1.07 g/cc0.0387 lb/in³Hardener; ASTM D-792
 1.07 g/cc0.0387 lb/in³Cure 1; ASTM D-792
 1.07 g/cc0.0387 lb/in³Cure 2; ASTM D-792
Viscosity 690 cP690 cPHardener; ASTM D-2393
 790 cP790 cPMix; ASTM D-2393
 1200 cP1200 cPResin; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inCure 1; ASTM D-2566
 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25 - 3525 - 35Cure 1; ASTM D-2240
 25 - 3525 - 35Cure 2; ASTM D-2240
Tensile Strength 1.72 MPa250 psiCure 1; ASTM D-638
 1.72 MPa250 psiCure 2; ASTM D-638
Elongation at Break 250 %250 %Cure 1; ASTM D-638
 250 %250 %Cure 2; ASTM D-638
Tear Strength 7.01 kN/m40.0 pliCure 1; ASTM D-624
 7.01 kN/m40.0 pliCure 2; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 480 min4.00 - 8.00 hourMix, Demold time
Gel Time 15.0 - 25.0 min15.0 - 25.0 minMix
 
Descriptive Properties
AspectClearCure 1
 ClearCure 2
Mix Ratio32:100Resin: Hardener, Weight
 32:100Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF109 / 317709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.