MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals H567JA High density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: SCG™ HDPE H567JA is a high density polyethylene resin with excellent processing performance and mechanical properties, especially for environmental stress cracking resistance. It is particularly designed for injection molding and continuous compression molding of beverage caps and closures. Related Finished Products: Caps and closures for carbonated soft drinks and hot fill beverages.

Applications: Beverage caps and closures: carbonated soft drink.

Features: Excellent process ability. Excellent environmental stress cracking resistance. Good mechanical property. Good organoleptic property.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D 1505
ESCR 10% Igepal® >= 600 hour>= 600 hourF50, condition B, compression molded; ASTM D1693
Linear Mold Shrinkage, Flow 0.030 cm/cm
@Thickness 2.00 mm
0.030 in/in
@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.0265 cm/cm
@Thickness 2.00 mm
0.0265 in/in
@Thickness 0.0787 in
TPE Method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.4 MPa4120 psicrosshead speed 50 mm/min; ASTM D638
Tensile Strength, Yield 24.5 MPa3550 psicrosshead speed 50 mm/min; ASTM D638
Elongation at Break 950 %950 %crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 1.03 GPa149 ksiASTM D790
Izod Impact, Notched 0.590 J/cm
@Temperature 23.0 °C
1.11 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FASTM D648
 
Descriptive Properties
AppearanceBlock pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC717 / 277974

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.