Titanvene™ HD5120EA-B is a high density polyethylene copolymer with a narrow molecular weight distribution, which has been specially developed for packaging of carbonated beverages and for other applications where very high environmental stress cracking resistance (ESCR) is required. Titanvene™ HD5120EA-B has excellent organoleptic properties that do not significantly transfer taste or odor to the packaged product. Titanvene™ HD5120EA-B is characterized by excellent impact strength and creep resistance. Applications: Titanvene™ HD5120EA-B is designed for bottle caps of non-carbonated beverages or other closures where very high ESCR is required. Information provided by Lotte Advanced Materials. |