System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Potters Industries Spheriglass® EMB-20 Low Alkaline Boro-Silicate Solid Glass Microspheres
Categories:
Ceramic
;
Glass
;
Oxide
;
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.
Information provided by Potters Industries.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
2.60
g/cc
0.0939
lb/in³
Particle Size
10
µm
10
µm
Mean
2.0
-
20
µm
2.0
-
20
µm
Mechanical Properties
Metric
English
Comments
Hardness, Mohs
6.5
6.5
Thermal Properties
Metric
English
Comments
CTE, linear
5.10
µm/m-°C
2.83
µin/in-°F
Thermal Conductivity
1.03
W/m-K
7.16
BTU-in/hr-ft²-°F
Softening Point
830
°C
1530
°F
Optical Properties
Metric
English
Comments
Refractive Index
1.53 - 1.57
1.53 - 1.57
Component Elements Properties
Metric
English
Comments
Al2O3
14 %
14 %
B2O3
5.7 %
5.7 %
CaO
23.1 %
23.1 %
Fe2O3
0.20 %
0.20 %
K2O
<= 0.50 %
<= 0.50 %
MgO
1.0 %
1.0 %
Na2O
<= 0.50 %
<= 0.50 %
SiO2
55.5 %
55.5 %
Descriptive Properties
Shape
spherical
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Potters Industries Spheriglass® 3000 Solid Glass Spheres
CHT Group QSil 7750 Addition Cure, Thermally Conductive Material
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant
Bismuth, Bi
CPOT9909 / 161899
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.