MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ ABS resins are thermoplastic material which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming processes. The automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosities, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 2.5 to 12 ft-lb/in and heat distortion temperatures from 165 to 190°F are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating. Within the MAGNUM ABS product line, MAGNUM 1150 EM ABS resin is a high impact, medium heat, low gloss resin. MAGNUM™ 1150 EM has improved low temperature impact strength over standard grades of ABS. MAGNUM™ 1150 EM is used in applications like pillars and instrument panel trim.

Automotive Specifications:

  • CHRYSLER MS-DB-198 Type B CPN3903 Color: 100% Color Match

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0070 in/inASTM D955
Melt Flow 0.90 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 36.5 MPa
@Thickness 3.20 mm
51 mm/min; ASTM D638
Elongation at Break 30 %
@Thickness 3.20 mm
51 mm/min; ASTM D638
Elongation at Yield 3.0 %
@Thickness 3.20 mm
51 mm/min; ASTM D638
Tensile Modulus 1750 MPa
@Thickness 3.20 mm
51 mm/min; ASTM D638
Flexural Strength 58.9 MPa
@Thickness 3.20 mm
5.1 mm/min; ASTM D790
Flexural Modulus 1980 MPa5.1 mm/min; ASTM D790
Izod Impact, Notched 340 J/m
@Thickness 3.20 mm,
Temperature -29.0 °C
ASTM D256
 560 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Dart Drop, Total Energy 29.9 J
@Thickness 3.20 mm,
Temperature 23.0 °C
Peak, 6.71 m/sec; ASTM D3763
 32.8 J
@Thickness 3.20 mm,
Temperature -29.0 °C
Peak, 6.71 m/sec; ASTM D3763
 42.9 J
@Thickness 3.20 mm,
Temperature -29.0 °C
6.71 m/sec; ASTM D3763
 45.2 J
@Thickness 3.20 mm,
Temperature 23.0 °C
6.71 m/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
@Thickness 3.20 mm
ASTM D969
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
 111 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
 108 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Vicat Softening Point 112 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 218 - 274 °C
Mold Temperature 27.0 - 60.0 °C
Drying Temperature 82.0 °C
Dry Time 2.00 - 4.00 hour
Back Pressure 1.03 - 3.45 MPa
Clamp Pressure 28.0 - 69.0 MPa
 
Descriptive Properties
Screw Compression Ratio1.5:1.0 to 3.5:1.0
Screw L/D Ratio20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond TR 5000
Envalior Arnitel® EL250 TPC-ET, Injection Molding
Trinseo CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant
Chevron Phillips EA3025 Crystal Polystyrene
Ineos ABS Centrex® 401 AES Extrusion

PDOW1396 / 30614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.