MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Enviro Tech International EnSolv® n-Propyl Bromide Vapor Degreasing Solvent
Categories: Fluid; Solvent

Material Notes: EnSolv is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane and other hazardous vapor degreasing and general use solvents for critical applications such as oxygen service, precision optics, medical devices, high vacuum components and electronics. EnSolv is a superior cleaner for oxygen service lines and components that leaves virtually no residue and conforms to SAE ARP1176. It is an excellent choice for removal of a wide range of organic soils by vapor degreaser, ultrasonic cavitation, dip tank, flushing or hand wiping. EnSolv is a patented azeotropic mixture that can be distilled and reused through numerous cycles before it needs to be replaced. EnSolv is compatible with all metals and many plastics and other materials typically cleaned in vapor degreasers, ultrasonic tanks or manually.

Information provided by Enviro Tech International.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.00512 g/ccVapor Density
 1.31 g/cc
@Temperature 23.9 °C
Water Absorption <= 0.020 %
Viscosity 0.49 cP
@Temperature 25.0 °C
Vapor Pressure 134 torr
@Temperature 25.0 °C
Surface Tension 25.9 dynes/cm200°C
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 21000 VAC
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 58.8 cal/g
Specific Heat Capacity 0.260 BTU/lb-°F
Boiling Point 70.0 °C
Decomposition Temperature >= 400 °C
Flammability Test 3.8 - 9.5vol% limits based on n-Propyl Bromide
 
Descriptive Properties
Acid Acceptance, as NaOH>0.19% by wt.
Acidity , as HCl< 0.0010% by wt.
AppearanceClear; free of suspended matter
Atmospheric Lifetimeabout 19 days
Base Materials Meets ASTM D6368Yes
Evaporation Rate (Butyl Acetate = 1)4.7
Flash Point TCCNone
Global Warming Potential (GWP)Almost zero (0.00005 - 0.0002)
Hansen Parameter Non-Polar16
Hansen Parameter Polar5.8
Hildebrand Parameter17.9
Kauri Butanol Number130
Ozone Depletion Potential (ODP)0.016

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Enviro Tech International EnSolv® 5408 n-Propyl Bromide Vapor Degreasing Solvent

WENSOL00 / 75422

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.