Extraction and lipid resistant, non-migrating for use in contact with polystyrene, polycarbonate, etc. Good melt flow, low processing temperatures, superior heat stability & good mold release for connectors, accessories to IV bags, catheters, etc. Formulated for injection molding or extrusionAlphagary is part of Orbia. |