MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plaskolite Vivak PETG Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details. It can be easily decorated by painting, silk screening or hot stamping. VIVAK is heavily used in the POP display and store fixture industries. VIVAK PETG is produced using resin that complies with FDA requirements for food contact applications. VIVAK is a transparent copolyester that offers a unique balance of physical properties and ease of fabrication.

Data provided by the manufacturer, Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D792
Water Absorption 0.2 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D285
Tensile Strength 7700 psiASTM D638
Tensile Modulus 320300 psiASTM D638
Flexural Strength 11200 psiASTM D790
Flexural Modulus 310 ksiASTM D790
Compressive Strength 8000 psiASTM D695
Shear Strength 9000 psiASTM D732
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.4
@Frequency 1e+6 Hz
ASTM D150
 2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 410 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µin/in-°F
@Temperature -34.4 - -1.11 °C
ASTM D696
Thermal Conductivity 1.56 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 164 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 157 °FASTM D648
Glass Transition Temp, Tg 178 °FASTM D3418
Flammability, UL94 HB
Flame Spread 0.0600 in/minASTM D635
Flame Spread Index 85ASTM E84
Ignition Temperature 880 °FSelf Ignition; ASTM D1929
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57
@Wavelength 589.3 nm
nD; ASTM D542
Haze 1.0 %ASTM D1003
Transmission, Visible 86 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Smoke Developed Index450ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite Mustang PETG Sheet
IPB Veralite® 200 Transparent PETG Sheet
Overview of materials for PETG Copolyester
Covestro Makrolon® FD sheet Polycarbonate
Röhm Plexiglas® 100 Resist® Extruded Acrylic

PPLAS902 / 150439

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.