MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lushan EP252 Adhesive Resin for Sewerage and Drainage Pipe
Categories: Polymer; Adhesive; Thermoplastic; Polyethylene (PE)

Material Notes: Adhesive resin Lushan EP252 is maleic grafted polyethylene. It’s mainly used for reinforced PE spiral corrugated steel pipes and steel wire with larger caliber. Adhesive resin Lushan EP252 solves the adherence problems between plastics and plastics, plastics and metal, glass and other materials. With super strong adhesion, wide application scope, excellent water and oxygen insulating properties, adhesive resin Lushan EP252 series provides a comprehensive solution for larger diameter steel pipe in drainage and sewerage pipe systems.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1505
Melt Index of Compound 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 115 °CASTM D1525
Brittleness Temperature -70.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 137 NA Performance Polypropylene Polymer
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
Ipiranga Petrochem GM 5250 OC HDPE
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes

PLUSH019 / 150017

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.