MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® C40 L Nylon 66/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Product Description: Ultramid® C40 L is a lubricated copolymer 66/6 grade of high viscosity for the production of high transparency, nonsymmetric blown film with reduced curl. Its very low melting point compared to standard PA6 is advantageous for co extrusion with temperature sensitive polymers like EVOH.

Availability: Europe; North America

Additive: Lubricant: 250 to 550 ppm

Features: Copolymer; High Clarity; High Viscosity; Lubricated

Uses: Blown Film; Monofilaments

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Forms: Pellets

Processing Method: Blown Film; Coextrusion

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.780 g/cc0.0282 lb/in³Apparent
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption 3.2 %3.2 %Equilibrium, 50% RH
Water Absorption at Saturation 11 %11 %
Particle Size 2000 - 2500 µm2000 - 2500 µmPellet size
Viscosity Measurement 3.89 - 4.173.89 - 4.171% in 96% Sulfuric Acid; ISO 307
Viscosity Number 240 - 260 cm³/g2.40 - 2.60 dl/gISO 307
 
Thermal PropertiesMetricEnglishComments
Melting Point 188 - 190 °C370 - 374 °FISO 3164
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %ISO 15512
 
Descriptive Properties
Extractables<0.8%ISO 6427

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2056 / 310749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.