MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAFORM C 904 UR POM-C
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: KEBAFORM C904 UR is a normal viscosity, elastomer-containing injection molding grade based on KEBAFORM C 90.0. The increased elastomer content results in a very high toughness level. The absorption capacity for high dynamic loads is excellent. Fields of application include outset technology, track rollers, belt buckles, transport chains, fastening elements, etc.

Properties: dimensionally stable, good chemical resistance, good gliding properties, good recovery behavior, impact resistant, semi-crystalline

Typical areas of application: Gears, Fasteners, Spring elements, Handles, Belt buckles, industrial goods, Bearing bushes, Outset technology, Pneumatic tubes, Rollers, Sports & Leisure Articles, shockproof housing, Transport chains, Valves, Connecting elements

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.0170 cm/cm0.0170 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0170 cm/cm0.0170 in/inISO 294-4
Melt Flow 7.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psiISO 527-1
Elongation at Break 50.0 %50.0 %ISO 527-1
Modulus of Elasticity 1.75 GPa254 ksiISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure 1.00 - 4.00 MPa145 - 580 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO643 / 326717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.