MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT SE2003 Silicone elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a 2-component, silicone elastomer specifically designed for electronic potting and encapsulation applications. It offers good protection against chemicals, environmental contamination, mechanical shock, vibration and impact damage. It can be applied in areas where low flammability is a prerequisite. The cured elastomer can be repaired. The component parts have relatively low viscosities and are easily mixed either by hand or machine.

Key Features

  • Room temperature cure
  • Non-corrosive
  • Excellent thermal conductivity
  • Resistant to reversion
Cured product: After 7 days at 23°C +/- 2°C and 50% +/- 5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.30 g/cc0.0831 lb/in³
Brookfield Viscosity 30000 cP30000 cPB
 35000 cP35000 cPMixed
 40000 cP40000 cPA
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inBS ISO 2781
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240-95
Tensile Strength 3.30 MPa479 psiISO 37
Elongation at Break 40 %40 %ISO 37
Tensile Modulus 0.0169 GPa2.45 ksiYoung's
Tear Strength 5.00 kN/m28.5 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+14 ohm-cm3.00e+14 ohm-cmASTM D-257
Surface Resistance 1.76e+15 ohm1.76e+15 ohmASTM D-257
Dielectric Constant 6.0
@Frequency 1000 Hz
6.0
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 22.5 kV/mm572 kV/inASTM D-149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 155 µm/m-°C86.1 µin/in-°F
Thermal Conductivity 1.27 W/m-K8.81 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 60.0 min60.0 min
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
AppearanceAddition
ColorBrick redCured Product
 RedB
 WhiteA
Mix Ratio1:1By Weight
RheologyViscous liquid
Self BondingNo
Volume Coefficient of Thermal Expansion465 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL059 / 314542

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.