MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Alfa Chemistry Materials Praseodymium Metal
Categories: Metal

Material Notes: It is an important alloying agent in Neodymium-Iron-Boron magnets. Praseodymium is used to create high-power magnets notable for their strength and durability. It also used in lighters, torch strikers, 'flint and steel' fire starters, etc. Praseodymium Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder. Praseodymium is a soft, silvery-yellow, malleable, ductile metal. More resistant to corrosion in air than some other rare earths, it develops a green oxide coating that spalls off when exposed to air. Praseodymium is never found free in nature, appearing only in combined form with other rare earths in various minerals. It should be stored under mineral oil or in an inert atmosphere. Similar to other rare earths, praseodymium forms brightly colored compounds.

Applications: is used as high-strength alloying agent in the magnesium used in parts of aircraft engines. It is an important alloying agent in Neodymium-Iron-Boron magnets. Praseodymium Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder, please visit Rare Earth Metals & Sputtering Targets page for more detailed information.

Solubility: Reacts with water

Molecular Formula: Pr

stored under mineral oil or in an inert atmosphereAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.71 g/cc0.242 lb/in³
Molecular Weight 141 g/mol141 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 931 °C1710 °F
Boiling Point 3520 °C6370 °F
 
Descriptive Properties
AppearanceSilvery white
CAS Number7440-10-0
Purity99.9% 99.5% 99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA66583 / 304705

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.