MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPC 2660 Polypropylene, Heterophasic Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properties.

Application

PPC 2660 is suitable for the extrusion of corrugated cardboard, blown film, sheet and pipes and for blow-molding applications where a very high impact resistance is required.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7474ISO 2039-2
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-2
Elongation at Yield 13 %13 %ISO 527-2
Tensile Modulus 1.20 GPa174 ksiISO 527-2
Flexural Modulus 1.10 GPa160 ksiISO 527-2
Izod Impact, Notched (ISO) 50.0 kJ/m²23.8 ft-lb/in²ISO 179
 6.00 kJ/m²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched >= 5.00 J/cm²>= 23.8 ft-lb/in²
 0.600 J/cm²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °F120°C per hour; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °F120°C per hour; ISO 75-2
Vicat Softening Point 60.0 °C140 °F50N-50°C per hour; ISO 306
 130 °C266 °F10N-50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EPD 60 R Polypropylene
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)
LG Chemical HI-151 ABS, Middle Impact
Total PPH 3429 Polypropylene, Injection Molding Grade
Total PPC 3640 Polypropylene, Heterophasic Copolymer

PFINAA079 / 38515

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.