MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Casting Alloy, UNS C87610, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Sand Cast

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding

Typical uses: Statuary; Decorative Pieces; Pump Components; Valve Stems

Applicable Specifications: As Sand Cast – Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  96
@Load 500 kg
96
@Load 1100 lb
 135
@Load 3000 kg
135
@Load 6610 lb
Hardness, Rockwell B 7676
Tensile Strength >= 310 MPa>= 45000 psifor Standard
 400 MPa58000 psiTypical
Elongation at Break >= 20 %>= 20 %for Standard
 35 %35 %Typical
Tensile Modulus 110 GPa16000 ksi
Compressive Strength 131 MPa19000 psi0.001 in. set/in.
 414 MPa60000 psi0.01 in. set/in.
Machinability 40 %40 %
Shear Strength 193 MPa28000 psi
Izod Impact 44.7 J33.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000280 ohm-cm0.0000280 ohm-cm6.1% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 µm/m-°C
@Temperature 20.0 - 300 °C
11.0 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 2.36 W/m-K16.4 BTU-in/hr-ft²-°F
Melting Point 821 - 971 °C1510 - 1780 °F
Solidus 821 °C1510 °F
Liquidus 971 °C1780 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 90 %>= 90 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.25 %<= 0.25 %
Silicon, Si 3.0 - 5.0 %3.0 - 5.0 %
Zinc, Zn 3.0 - 5.0 %3.0 - 5.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC87610x2 / 293183

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.