MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chi Mei Acryrex® PG-383D Optical Grade PMMA Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded

Material Notes: Optical grade resin with low melt volume-flow rate. Applications: Widely used in optical extrusion applications. Raw material used to make the diffuser for LCD back-lights.

ACRYREX® Optical PMMA Resin is made with 99% methyl methacrylate (MMA) and 1% additives. It features good cleanliness, weather resistance, heat resistance, transparency, and gloss. It also exhibits stable physical, chemical, optical, and electrical properties. ACRYREX® Optical Grade PMMA Resin is widely used in the application of optical grade light guide plates, lighting signage, and backlight modules.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Melt Volume Rate (ml/10 min.); ISO 1133
ASTM Color -2.00ASTM E 308
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 54.0 MPa50 mm/min; ISO 527
Elongation at Break 6.0 %50mm/min; ISO 527
Flexural Strength 82.0 MPa2mm/min; ISO 178
Flexural Modulus 82.0 GPa2mm/min; ISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 106 °C
@Load 1.00 kg
50°C/hr; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHI9915 / 280800

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.