MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Kane TIGERLAC™ 5061 Shellac
Categories: Other Engineering Material

Material Notes: TIGERLAC™ Flaked Shellacs are dewaxed and physically decolorized natural resins. The single products differ in the degree of decolorization and yield transparent solutions of different color shade in various solvent systems. Ready for use solutions of the product are available. The TIGERLAC™ Flaked Shellac manufacturing process guarantees careful treatment of the natural raw materials (seedlac) upon refining. The final products are high quality materials with excellent binding and film forming properties. They are physiologically harmless and biodegradable.

Major Applications: Wood coatings and glazes, flexographic printing inks, India inks, leather finishing, hat proofing, cosmetics (e.g. hair sprays, shampoos), confectionary and fruit coatings, direct food contact materials (packagings), raw material for shellac special products.

Information provided by Kane International Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value 60 - 7560 - 75
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 - 77.0 °C149 - 171 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month
@Temperature <=20.0 °C
24.0 Month
@Temperature <=68.0 °F
 
Descriptive Properties
Color> 9Index Lovidbond PRS Scale (20%) in ethanol)
KosherO.U. Parve
Loss on drying< 2%
Saponification Value175 - 240 mg KOH/g
Wax content< 0.2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKKANE007 / 295540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.