MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemours Teflon™ FFR 750 Fluoroplastic Foam Resin
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Teflon™ FFR 750 is a fluoroplastic resin compounded with a foam nucleating package. This resin is supplied as white pellets and is used in a nitrogen gas-injected foam extrusion process to produce uniform foam cells in the dielectric insulation. Foaming the fluoroplastic reduces its dielectric constant, providing opportunities for miniaturization and weight savings. Foamed insulation of Teflon™ FFR 750 produces cables for high frequency signal transmission with minimal distortion. Teflon™ FFR 750 is ideal for producing coaxial cable cores in a broad range of sizes.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.14 g/cc2.14 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 372 °C
12 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D2116
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.04
@Frequency 1000 Hz
2.04
@Frequency 1000 Hz
ASTM D150
 2.04
@Frequency 1e+6 Hz
2.04
@Frequency 1e+6 Hz
ASTM D150
 2.04
@Frequency 1e+9 Hz
2.04
@Frequency 1e+9 Hz
ASTM D2520
Dissipation Factor  0.00010
@Frequency 1000 Hz
0.00010
@Frequency 1000 Hz
ASTM D150
 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
ASTM D150
 0.00040
@Frequency 1e+9 Hz
0.00040
@Frequency 1e+9 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 - 290 °C500 - 554 °FASTM D4591

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8796 / 268722

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.