MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zotefoams ZOTEK® F OSU Rigid PVDF Foam
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

This grade is ideal for soft trim in combination with leathers, textiles and decorative laminates, including low FST cores for composites and divider panels.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0740 g/cc0.00267 lb/in³ISO 845
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.00 MPa145 psiISO 1798
Elongation at Break 90 %90 %
Compressive Yield Strength 0.150 MPa
@Strain 25 %
21.8 psi
@Strain 25 %
ISO 7214
Compression Set 20 %
@Time 79200 sec,
Strain 50 %
20 %
@Time 22.0 hour,
Strain 50 %
0.5 hr recovery; ISO 7214
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0323 W/m-K0.224 BTU-in/hr-ft²-°Fmean temp of 0°C; ISO 8301
 0.0369 W/m-K0.256 BTU-in/hr-ft²-°Fmean temp of 50°C; ISO 8301
 0.0416 W/m-K0.289 BTU-in/hr-ft²-°Fmean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 157 °C315 °F
 
Descriptive Properties
FlammabilityHeat Release: FAR/CS 25.853, 2 min totalPass at 13 mm
 Heat Release: FAR/CS 25.853, PeakPass at 13 mm
 Radiant Heat Panel: FAR 25.856Pass at 3, 13, and 25 mm
 Smoke Density: ABD0031Pass at 13 mm
 Smoke Density: FAR/CS 25.853Pass at 13 mm
 Toxic Gas Emission: ABD0031Pass at 13 mm
 Vertical Burner (60 sec): FAR/CS 25.853Pass at 25 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zotefoams ZOTEK® F OSU Flexible PVDF Foam
Zotefoams ZOTEK® F 74 HT PVDF Foam
Zotefoams ZOTEK® F 40 HT PVDF Foam
Zotefoams ZOTEK® F 40 HT LS PVDF Foam
Zotefoams ZOTEK® F 35 PVDF Foam

PZOTEF961 / 150717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.