MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Plastic Lumber from the Plastic Lumber Co.  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Wood and Natural Products; Wood

Material Notes: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained acceptance with governments, commercial entities and individuals where no maintenance and durability are of the utmost importance.

Information provided by The Plastic Lumber Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 - 0.980 g/ccASTM D792
 35.6 lb/ft³ASTM D6111-97
Water Absorption <= 0.010 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
Tensile Strength at Break 1470 - 1700 psi
Modulus of Elasticity 115 ksi
Flexural Yield Strength 1000.8 psiStress at 3% Strain; ASTM D6109-97
Compressive Strength 1337.4 psiStress at 3% Strain; ASTM D6108-97
Compressive Modulus 0.4713 GPaCompressive Secant Modulus; ASTM D6108-97
Secant Modulus 0.3437 GPaFlexural Secant Modulus; ASTM D6109-97
Izod Impact, Unnotched 2.80 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 10.0 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Melting Point 225 °C
Flash Point 330 °CASTM E138
 
Descriptive Properties
Compressive Strength3200-3800 lb/in
Nail Withdrawal140 lbs6 Penny Common Bright
Screw Withdrawal350 lbs#10 by 1 inch

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carbon-Core Carbon Balsa Wood
3M Balsa Panels
Plywood
DIAB ProBalsa® PB Standard Balsa Wood
Douglas-fir Plywood

PLUMBER0 / 52058

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.