MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ketron® TF20 PEEK SP Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Compared with Ketron® 1000 PEEK SP this PTFE filled PEEK SP grade offers improved frictional properties (considerably reduced coefficient of friction) and higher pressure-velocity capabilities.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccISO 1183-1
Water Absorption 0.050 %
@Time 86400 sec
immersion in water; ISO 62
Water Absorption at Saturation 0.38 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88ISO 2039-2
Tensile Strength 73.0 MPaISO 527-1/-2
Elongation at Break 5.0 %ISO 527-1/-2
Modulus of Elasticity 3.40 GPaISO 527-1/-2
Compressive Strength 29.0 MPa
@Strain 1 %
ISO 604
 56.0 MPa
@Strain 2 %
ISO 604
 100 MPa
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched 30.0 kJ/m²ISO 179-1/1eU
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistivity per Square 1.00e+13 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 23.0 - 100 °C
 65.0 µm/m-°C
@Temperature 23.0 - 150 °C
 150 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.250 W/m-K
Melting Point 340 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75-1/-2
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 V-0
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM904 / 291061

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.