MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Silicon Carbide, Alpha SiC
Categories: Ceramic; Carbide

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/ccsintered
 3.21 g/cccrystalline
a Lattice Constant 3.0817 Å
c Lattice Constant 15.1183 Å
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 410 GPasintered
Compressive Strength 4600 MPasintered
Poissons Ratio 0.14sintered
Fracture Toughness 4.60 MPa-m½sintered
Shear Modulus 180 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.00000640Atomic (cgs)
Dielectric Constant 10.2
Band Gap 2.86 eV
Electron Mobility, cm²/V-s 400
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.670 J/g-°Csintered
Thermal Conductivity 77.5 W/m-K
@Temperature 400 °C
sintered
 125.6 W/m-K
@Temperature 200 °C
sintered
Melting Point 2797 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.67
 
Descriptive Properties
CAS Number409-21-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, CVD
Silicon Carbide, sublimed
Silicon Carbide, Reaction-Bonded, SiSiC
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Tungsten Carbide, WC

BCSC2A / 160

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.