MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Wacker® F 1006 Fluid
Categories: Fluid; Polymer

Material Notes: F1006 is a clear, colorless polydimethyl siloxane fluid having silanol group in the terminal position. Due to the silanol groups F1006 reacts with itself or with functional silanes in a condensation reaction. The silanol fluids react with Si-H containing fluids by evolution of hydrogen.

Application: The reactive F1006 is suitable for intermolecular crosslinking for achieving the desired increase in elasticity. Reactive silicones serve not only to improve the properties of the material, but also the processing conditions. For example, they are used in the finishing of jeans and in pigment printing. F1006 may be used to impart hydrophobicity to silica. For example, it can be mixed with silica at 0.5% to 10% weight level.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 - 4.0 %WSTM 3359
Viscosity 55 - 120 cPWSTM 3018
 
Descriptive Properties
Color0-30Alpha, WSTM 3004
Content1-2%OH as SiOH by FTIR, WSTM 7233

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9765 / 205294

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.