MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Titan Plastics Titalon 1C00MGF Nylon 6, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Product Description: Glass Fiber Reinforced, High Thermal Conductivity Specifications

Information provided by Titan Plastics Compounds co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/in50x70x3 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 92.0 MPa13300 psiISO 527 1,2
Elongation at Break >= 2.0 %>= 2.0 %ISO 527 1,2
Flexural Strength 120 MPa17400 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 1.00e+10 ohm-cm1.00e+7 - 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+7 - 1.00e+10 ohm1.00e+7 - 1.00e+10 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 3.60 W/m-K25.0 BTU-in/hr-ft²-°FThrough plane; ISO/DIS 22007-2
 20.0 W/m-K139 BTU-in/hr-ft²-°Fin plane; ISO/DIS 22007-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75 1,2
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Injection Velocity 50.0 - 60.0 mm/sec1.97 - 2.36 in/sec
Drying Temperature 90.0 °C194 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Injection Pressure 50.0 - 70.0 MPa7250 - 10200 psi
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTITP012 / 281642

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.