MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Rulon® FCJ Bearing/Seal PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.

Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion.

FCJ: Identical composition to RULON CJ except the innermost layer is a RULON F tape liner instead of the synthetic fiber/PTFE liner. Ideally suited for non-lubricated moderate-load/high-speed applications that require a low coefficient of friction. Rc 25 and higher steel mating surface. Material has thermal and electrical insulating properties. Suitable for use in wet, dry, or vacuum environments. Markets for FCJ grade include Agricultural, Appliances, Automotive, Construction, Industrial, Transportation.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
Immersion
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 138 MPa20000 psiMax load under tribological use
Compressive Strength 345 MPa50000 psi
Izod Impact, Notched 7.47 J/cm14.0 ft-lb/in
Limiting Pressure Velocity 0.701 MPa-m/sec20000 psi-ft/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.40e+18 ohm-cm2.40e+18 ohm-cm
Surface Resistance 3.90e+15 ohm3.90e+15 ohm
Dielectric Constant 4.15
@Frequency 1e+6 Hz
4.15
@Frequency 1e+6 Hz
Dielectric Strength 7.87 kV/mm200 kV/inShort Term
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 µm/m-°C7.00 µin/in-°F
Thermal Conductivity 0.202 W/m-K1.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C350 °F
Deflection Temperature at 1.8 MPa (264 psi) 177 °C350 °F
Minimum Service Temperature, Air -196 °C-320 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® ACM Bearing/Seal PTFE
TriStar TriSteel PT Metal Backed PTFE Bearing System
Saint-Gobain Rulon® J Bearing/Seal PTFE
Saint-Gobain Rulon® II Bearing/Seal PTFE
Saint-Gobain Rulon® AR Bearing/Seal PTFE

PSTGQZ182 / 68696

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.