MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bearing Bronze, UNS C93700, Copper Casting Alloy, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Centrifugal Cast

Fabrication Properties: Good Suitability – Brazing, Soldering

Typical uses: Brackets; Nuts; Washers for Engines; Applications Requiring Acid Resistance to Sulphite Fluids; Bearing Plates; Bearings; Bushings; Bushings for high speed and heavy pressure.; Corrosion Resistant Castings; Crank Shafts; High Speed, Heavy Load Bearings; Impellers; Machine Parts; Parts for Steel Mill Maintenance; Pressure Tight Castings; Pumps; Slide Guides for Steel Mills Large Bearings for Ships

Applicable Specifications: As Centrifugal Cast – Castings SAE J461, Castings AMS 4842, Castings SAE J462, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings AMS 4842, Castings ASTM B763/B763M, Castings SAE J462, ASTM B66, Castings SAE J461, Castings ASTM B584, Castings ASME SB584, Castings ASTM B22/B22M; Bearings & Busings AMS 4827; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 30.0 ksifor Standard
Tensile Strength, Yield >= 12.0 ksifor Standard, 0.5% Ext
Elongation at Break >= 15 %for Standard
Tensile Modulus 11000 ksi
Machinability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000172 ohm-cm10% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 27.1 BTU-in/hr-ft²-°F
Melting Point 600 °FIncipient
 1403 - 1705 °F
Solidus 1403 °F
Liquidus 1705 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.50 %
Copper, Cu 78 - 82 %
Iron, Fe <= 0.70 %
Lead, Pb 8.0 - 11 %
Nickel, Ni <= 0.50 %
Phosphorus, P <= 0.10 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.080 %
Tin, Sn 9.0 - 11 %
Zinc, Zn <= 0.80 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC93700x1 / 293228

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.