MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Low Density (LDPE)

Material Notes: The Trilene® TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of films with uniform thickness and good visual appearance and weldability. This product presents excellent puncture resistance, exactly to the low temperatures, what it becomes it especially adequate the production of packings for frozen products, as cuts of meat and chicken with or without bone, fish, seafood and ice. The additive package gives it thermal stability, low blocking, and adequate slip performance, which are indispensable to allow high productivity on the extrusion, printing, and finishing lines. The resin should be processed in extruders that are designed or adapted for LLDPE. The components that form the product Trilene® TS 8056 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical laminated films designed for packaging of various products such as coffee, crackers, etc. Technical films for automatic or semi-automatic packaging of solid products (grains, powdered, etc.), liquids (milk, yogurt, etc.), and frozen foods (poultry, beef cuts, seafood, ice, etc.).

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 790 %ASTM D882
Film Elongation at Break, TD 890 %ASTM D882
Secant Modulus, MD 0.0930 GPa5%; ASTM D882
Secant Modulus, TD 0.0970 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.090ASTM D1894
Elmendorf Tear Strength, MD 13.2 g/micronASTM D1922
Elmendorf Tear Strength, TD 13.2 g/micronASTM D1922
Dart Drop Test 300 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 32.0 MPaASTM D882
Film Tensile Strength at Break, TD 29.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 7.5 %ASTM D1003
Gloss 113 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 190 °CPlasticizing Zone
 190 - 200 °CMixture Zone
Feed Temperature 170 - 180 °C
Adapter Temperature 180 - 200 °C
Die Cooling Temperature 200 - 220 °C
Die Opening 0.180 - 0.250 cm
Blow-up Ratio (BUR) 3.0Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Proportion LLDPE %75PTN-570-Q

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
ExxonMobil ESCOREZ™ 2173 (Europe) Petroleum Hydrocarbon Resin

PDAX109 / 29534

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.