MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tipco Tipwood® 50 EX 50EX
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Wood Filled

Material Notes: Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.

Features:

  • Environmentally Friendly Material
  • Easy Recyclability
  • 45-50% Special Wood Filler
  • Excellent Extrudability
  • High Melt Strength
  • Superior Draw Down for Vacuum/Thermo Formability
  • Wood-Like Surface Aesthetics
  • Good Izod Impact Strength
  • High Stiffness & Good Durability
  • Good Sound Barrier Properties
  • Extremely Low Thermal Sag

Applications: Sheet Extrusion, Thermoforming, Profiles, Blow Molding and Lamination. Automotive Car Interiors, Door Panels, Trims, Wood-Finish Panels, Office Files, Trays, Marine Flooring, Audio Speakers, Resonator Devices, Blow Molded Bottles, Furniture, Mono-Block Chairs and various Artificial Wood Products.

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D1505
Linear Mold Shrinkage, Flow 0.0080 cm/cmType I; ASTM D955
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3555.8 psiASTM D638
Elongation at Break 8.0 %ASTM D638
Flexural Modulus 355600 psiASTM D790
Izod Impact, Notched 0.64288 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 225 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 5 - 7 hourUse immediately after drying.
Moisture Content 0.25 %ASTM D817
Shelf Life 3.00 Monthat 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY WPE 2000 Wood Filled HDPE
GEHR Plastics ECO-GEHR® WPC-30PP Composite of 70% Wood Fibers and 30% Polypropylene (PP)
LyondellBasell Moplen EF300N Polypropylene, Impact Modified; Molded/Extruded
Overview of materials for Polypropylene, Fiber Grade
Overview of materials for Polystyrene, Wood Filled

PTIP605 / 70326

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.