MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 785 FG Parting Lubricant
Categories: Fluid; Lubricant

Material Notes: A white soft-paste, formulated with proprietary blend of ultra-fine inorganic solids lubricants, is a high quality thread lubricant and assembly paste. 785 FG is manufactured with ingredients that meet FDA requirements for incidental food contact. Because 785 FG Parting Lubricant utilizes a synthetic con-carbonizing base, the product can be used over a broad temperature range. Hardening will not occur when used between -34°C to 1204°C (-30°F to 2200°F).

Features:

  • No Toxic Heavy Metals
  • Non-staining, White color
  • Water and chemical resistant
  • Broad service temperature range
  • Balanced coefficient of friction
  • Ultra-fine particles
  • Contains no PTFE
  • NSF H1, Registration # 132237
  • Conforms to FDA 21 CFR 178.3750

Benefits:

  • Safer to workers
  • Usable under most extreme conditions
  • Fills microscopic voids in metal surfaces
  • Prevents galling of stainless steel and aluminum assemblies
  • Aids press fit assemblies.

Applications: 785 FG is made of ingredients conforming to applicable FDA standards for direct or incidental food contact. It is NSF registered H1 and is suitable for use in federally inspected meat and poultry plants. It is ideal where a white, non-staining lubricant is required, including textile, and pulp and paper applications. Suggested uses include all types of processing equipment where incidental food contact can occur:

  • Bottle filling equipment
  • Canning-filling machinery
  • Canning and bottling machinery
  • Carton – filling machines
  • Paste and sauce fillers
  • Meat – packing equipment
  • Fruit feeders
  • Bakery equipment

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/cc
Particle Size <= 25 µm<= 25 µm
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic 0.150.1540 kgf, 1200 rpm; ASTM D2266
Penetration P(0), 1/10 mm 360360[mm], Unworked; ASTM D217, ISO 2137
 370370[mm], Worked; ASTM D217, ISO 2137
K Factor (Wear Factor) 0.190.19
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1204 °C2199 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Dropping Point >= 225 °C>= 437 °FASTM D566, ISO2176
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ColorWhite
ConsistencySoft Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Portland Cement
Human Enamel (Canine)
Human Dentin (Molars)
Human Dentin (Canine)
Chesterton 690 FG Lubricant

PPTCHS095 / 138207

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.