MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bisalloy Steels BisPlate HHA Thickness 5-25 mm
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: A quenched and tempered steel armor plate suitable for use in both military and civil applications where light weight and resistance to ballistic projectiles is required.

Key Words: MIL-A-46100
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 500
Tensile Strength at Break 1640 MPa
Tensile Strength, Yield 1400 MPa
@Strain 0.2 %
Elongation at Break 14 %in 50 mm GL
Charpy Impact 8.00 - 16.0 J
@Temperature -20.0 °C
Transverse
 10.0 - 20.0 J
@Temperature -20.0 °C
Longitudinal
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.0020 %
Carbon, C 0.32 %
Chromium, Cr 1.2 %
Iron, Fe 97 %As Balance
Manganese, Mn 0.40 %
Molybdenum, Mo 0.30 %
Nickel, Ni 0.35 %
Phosphorus, P 0.025 %
Silicon, Si 0.35 %
Sulfur, S 0.0050 %
 
Descriptive Properties
CE (IIW)0.61
PCM0.4
Surface FinishShotblasted

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 546 Boron Carbide
3M Techical Ceramics Ekasic® C Silicone Carbide
Astralloy MIL-DTL-46100E Armor Steel Plate
ASTM A36 Steel, plate
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

NBISAL17 / 15464

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.