MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco 40 White Oil
Categories: Fluid; Lubricant; White Mineral Oil (WMO)

Material Notes: Texaco White Oils 40 delivers value through:
  • Nonstaining — Colorless, odorless, tasteless and nonstaining. The purity of Texaco White Oil 40 makes it the preferred choice for applications calling for a clean, nonstaining oil.

Texaco White Oil 40 is a colorless, odorless, tasteless mineral oil that is virtually free of nitrogen, sulfur, oxygen, and aromatic hydrocarbons. It contains Vitamin E, a natural antioxidant, to protect quality during handling and storage. It is clear, bright, and free of solids and water.

Texaco White Oil 40 is recommended for applications requiring a nonstaining, light viscosity oil.

Recommendations include:

  • Textile industry, such as twister rings, sewing and knitting machines
  • Paper industry, as a slitter oil
  • Other industries which require a nonstaining oil

Texaco White Oil 40 meets U.S. Pharmacopeia (USP) requirements for mineral oils.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220538; MSDS Number: 10324

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 31.6 °31.6 °
Saybolt Viscosity at 100°F 209 SUS209 SUS
Kinematic Viscosity at 40°C (104°F) 40.5 cSt40.5 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °F
Flash Point 210 °C410 °F
 
Descriptive Properties
Color30Saybolt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubriplate FMO 1100 AW USP Mineral Oil-Based Food Machinery Grade Oil
Lubriplate Flush Pure USP Mineral Oil-Based Food Machinery Grade Oil
Lubriplate FB 150 USP Mineral Oil-Based Food Machinery Grade Oil

WTEXA233 / 77112

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.