MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lotte Advanced Materials TITANEX MF1461 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MF1461 is a pelleted linear low density polyethylene Hexene-1 resin for blown film extrusion.

Applications: Geomembrane, High strength film.

Advantages: High melt strength, Excellent stress crack resistance, Excellent drawdown properties for high quality thin film.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ISO 1183 Method D
ESCR 10% Igepal® >= 4000 hour>= 4000 hourF50; ASTM D1693
Oxidative Induction Time (OIT) >= 130 min
@Temperature 200 °C
>= 130 min
@Temperature 392 °F
ASTM D3895
Melt Flow 0.100 g/10 min0.100 g/10 minI2; ASTM D1238
 14.0 g/10 min14.0 g/10 minI21; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 310 MPa45000 psiASTM D638
Elongation at Break 700 %700 %ASTM D638
Flexural Modulus 1.02 GPa148 ksiISO 178
Izod Impact, Notched (ISO) 58.0 kJ/m²27.6 ft-lb/in²ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9614 / 326096

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.