MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.

Unfilled Extrusion Resins
Akulon resins are available with melt viscosities to suit all extrusion processes: barrier and coating film, tube and hose, monofilament, stock shapes. Akulon resins are characterized by:

  • consistent quality
  • high purity
  • for film applications, low gel contents.

Molding Resins
Suited to all engineering demands:

  • Unfilled low and medium viscosity grades
  • Toughened unfilled grades
  • Glass reinforced from 20-45% filled
  • Low warpage reinforced grades
  • Flame retardant; UL V0 rated and glow wire types
  • Halogen free FR grades
  • Blow moldable materials
  • Laser markable resins
  • Laser weldable, high burst pressure grades
  • Toughened, reinforced resins
  • High stiffness grades for metal replacement

Akulon Ultraflow resins have high flow with mechanical properties similar to standard materials. Exceptional flow allows:

  • productivity gains in molding
  • lower built in stresses
  • better surface appearance
  • system cost reductions

Applications for Molding resins There is an Akulon resin available suitable for any application requiring polyamides. Key areas where DSM has specific application knowledge are

  • Automotive
    • Under the hood and engine components
    • Exterior and interior applications
    • Electrical components and connectors
  • Electrical
    • Low voltage power distribution
    • Lighting
    • Power connectors
  • Consumer Durables
    • Power and lawn and garden tools
    • Small Appliances
    • Sports and leisure equipment
    • Furniture accessories
    • Industrial Goods
    • Transportation (railways)

Information provided by DSM.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 6.0 %Sim. to ISO 62
Moisture Absorption at Equilibrium 1.6 %Humidity Absorption; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527-1/-2
Elongation at Break 3.0 %ISO 527-1/-2
Tensile Modulus 9.50 GPaISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243-1
Dissipation Factor 0.0090
@Frequency 100 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 0.710 mm
IEC 60695-11-10
 
Descriptive Properties
Heat stabilized or stable to heatYes
Injection MoldingYes
Release agentYes
With fillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled
Envalior Akulon® S223-HG6 (Cond.) 30% Glass Reinforced Nylon 66 (North America)
Envalior Akulon® S223-HG6 PA66-GF30, Dry, 30% Glass Filled, Heat Stabilized
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT

PDSMA164 / 31043

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.