MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 230 Crystal Clear Sealant
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: 3M™ Crystal Clear Sealant 230 is a one component thermoplastic elastomer which forms permanent elastic bonds when used in surface sealing applications. 3M Crystal Clear Sealant 230 bonds to a wide variety of materials including plastics, metals, fiberglass, and wood. 3M Crystal Clear Sealant 230 is crystal clear after drying and has good UV resistance, plus has broad substrate adhesion for a wide range of productivity enhancement application

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/cc
Volatile Organic Compounds (VOC) Content 158 g/l
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25 - 35ASTM C661
Elongation at Break 300 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 117 °C
Minimum Service Temperature, Air -37.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 minSkin-Free, 50% RH
Tack-Free Time <= 20.0 min50% RH
Shelf Life 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite
SMAC SMACSONIC® Classic ST Noise and Vibration Damping
SMAC SMACFOAM® 1250S-01 Damping Material
SMAC BARRIER® Damping Material
LyondellBasell Hostacom DRS 1017T T BLACK Polypropylene, Impact Modified

PMM33142 / 167889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.