Radiation cross-linkable, flame retardant compound for insulation and sheathing applications Compound class: Insulation / sheathing Compound category: RDX Flame retardant: Halogenated Standards: UL 3288, 3289, 3321, 3398, 3456, 3470, 3505, and 3575; CSA CL 1503; SAE J-1127 STX; CSA AWM I A/B Typical applications: This compounds results in an extremely smooth surface, while still showing an extrudability at high speeds. The high temperature rating makes this compound an ideal choice for the insulation of heat-resistant wires and cables for applications in areas where wires and cables should withstand the high temperatures in small compartments. Features: Flame retardant; Flexible at low temperatures; Oil resistant; High temperature resistant; Flexible; Weather/UV resistant Information provided by Melos |