MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TECHNYL® A 218G V30 PA66, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.

Available in: Europe and Latin America

Product Applications: TECHNYL® A 218 V43 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry for engine components. This product is available in black. TECHNYL® A 218G V30 is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as:-cooling and heating radiator systems, header tanks, thermostat components, inlet/outlet pipes. This product is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527 Type 1A
Elongation at Break 4.0 %4.0 %ISO 527 Type 1A
Tensile Modulus 7.50 GPa1090 ksiISO 527 Type 1A
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inIEC 60243
Dissipation Factor 0.110.11IEC 60250
Comparative Tracking Index 425 V425 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY

PRHOD660 / 137891

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.