MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ho Hsiang Ching H-115C SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: This material is transparent with super soft, which is similar to the texture of skin. Its shockproof effect may reduce the impact of the crash to as touching the ground, particularly with bigger or bouncy actions. The outstanding shockproof features form the buffer and slow down the uncomfortable feeling by the impact. Since it has first-rate properties, this Class is used a lot in insoles and always becomes the best choice for footwear manufacturers.

Color: Transparent

The optimum combination of materials: PP, PE, EVA

Processing: Injection, Extrusion

Applications: Rehabilitation ball, Fitness equipment

Information provided by Ho Hsiang Ching Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 125 °C
20 g/10 min
@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore C 9.09.0ASTM D2240
Tensile Strength 0.588 MPa85.3 psiASTM 412C
Elongation at Break 1200 %1200 %ASTM 412C
Tear Strength 2.94 kN/m16.8 pliASTM 412C
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 351 °F
Middle Barrel Temperature 166 - 182 °C331 - 360 °F
Front Barrel Temperature 177 - 191 °C351 - 376 °F
Nozzle Temperature 182 - 204 °C360 - 399 °F
Mold Temperature 16.0 - 66.0 °C60.8 - 151 °F
Injection Velocity 13.0 - 25.0 mm/sec0.512 - 0.984 in/sec
Injection Pressure 34.0 - 69.0 MPa4930 - 10000 psi
Hold Pressure 14.0 - 48.0 MPa2030 - 6960 psi
Back Pressure 0.340 - 0.690 MPa49.3 - 100 psi
Screw Speed 50 - 70 rpm50 - 70 rpm
 
Descriptive Properties
Cold resistance temperature-40°C
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHSIANG027 / 312503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.