MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Description: ACN 102 is hi-tech compounded Acrylic Resin. This hi-composite is produced by Nano-Technology and used widely in paint and Coating industry

    Advantages:
  • High abrasion and corrosion resistance
  • High UV resistance
  • High scratch resistance
  • Outstanding surface appearance
    Certification:
  • ISO 9001:2008
  • Iranian Nano Technology Initiative Council Certification
    Application:
  • Traffic Marking Paint

Information provided by Asia Technology Pioneers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccASTM D1475
Solids Content 60 %60 %ASTM 1259
Viscosity 15000 - 25000 cP15000 - 25000 cPASTM D562
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 10<= 10
 
Mechanical PropertiesMetricEnglishComments
Abrasion 0.0230.023[Gr], 33% improvement; ASTM D4060
 
Descriptive Properties
Impedance AnalysesWater uptake ~ 10
Salt Spray ResistanceHigh ImprovedASTM 117
SolventToluene
Thermal behaviorsHigh Improved

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTATP06 / 135224

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.